MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult injection molding applications. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.

Key Features:

  • Non-hygroscopic product, requires little to no drying before processing.
  • Neutral, easy coloring formulation.
  • Recommended for applications requiring excellent ozone resistance.
  • Used in sealing applications.
  • Recommended for applications requiring excellent flex fatigue resistance.
  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification.
  • EU and China RoHS compliant.
Applications:
  • Automotive – Grips, HVAC Flapper Door Seals, Interior, Interior Mat, Weather Seals, Electronics, Floor Care, Kitchen Tools, Soft Touch Grips and Consumer Applications
  • Seals and Gaskets
Uses:
  • Automotive Applications
  • Cell Phones
  • Consumer Applications
  • Flexible Grips
  • Seals
Processing Method: Injection Molding and Multi Injection Molding

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc0.930 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545.12 in; ASTM D2240
 4747Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 3.23 MPa468 psiAir at 302°F, 168 hr; ASTM D573
 3.59 MPa520 psiAcross Flow; ASTM D412
Tensile Strength, Ultimate 1.52 MPa220 psiAcross Flow; ASTM D412
Tensile Stress at Strain 1.50 MPa
@Strain 100 %
218 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 303.4 %303.4 %Air at 302°F, 168 hr; ASTM D471
 410 %410 %Across Flow; ASTM D412
Compression Set 25 %
@Temperature 70.0 °C,
Time 79200 sec
25 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -62.2 °C-80.0 °FASTM D746
UL RTI, Electrical 100 °C212 °FUL 746
UL RTI, Mechanical with Impact  90.0 °C
@Thickness 1.10 mm
194 °F
@Thickness 0.0433 in
UL 746
 95.0 °C
@Thickness 3.00 mm
203 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 1.10 mm
HB
@Thickness 0.0433 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Rear Barrel Temperature 177 - 191 °C351 - 376 °F
Middle Barrel Temperature 179 - 193 °C354 - 379 °F
Front Barrel Temperature 185 - 199 °C365 - 390 °F
Nozzle Temperature 185 - 210 °C365 - 410 °F
Melt Temperature 143 - 216 °C289 - 421 °FProcessing
Mold Temperature 10.0 - 51.7 °C50.0 - 125 °F
Moisture Content 0.080 %0.080 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Clamp Pressure 41.4 - 68.9 MPa6000 - 10000 psi
Vent Depth 0.00254 cm0.00100 in
Cushion 0.317 - 0.635 cm0.125 - 0.250 in
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
ColorNatural Color
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer

PADVA010 / 22700

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.