MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celcon® WR25Z POM, UV Resistant
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Celcon« WR25Z is a 2.5 nominal melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications. Celcon« WR25Z is a lower flow product providing improved toughness. Available in black only.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.016 cm/cm0.016 in/inISO 294-4
 0.022 cm/cm0.022 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/inASTM D955
 0.018 cm/cm0.018 in/inISO 294-4
Melt Flow 2.5 g/10 min2.5 g/10 minASTM D1238
 2.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.7 MPa8800 psiASTM D638
 61.0 MPa8850 psi50mm/min; ISO 527-2/1A
Elongation at Yield 10 %10 %50mm/min; ISO 527-2/1A
Tensile Modulus 2.60 GPa377 ksi50mm/min; ISO 527-2/1A
Flexural Modulus 2.55 GPa370 ksiISO 178
 2.59 GPa375 ksiASTM D790
Izod Impact, Notched 0.747 J/cm1.40 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 6.20 kJ/m²2.95 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.640 J/cm²3.05 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
Melting Point 165 °C329 °FASTM D3418
 166 °C331 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C198 °FISO 75-1, -2
 110 °C230 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
 180 - 200 °C356 - 392 °Fhot runner
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 180 - 190 °C356 - 374 °F
Zone 4 190 - 200 °C374 - 392 °F
Die Temperature 190 - 200 °C374 - 392 °F
Melt Temperature 180 - 200 °C356 - 392 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 3.00 hour3.00 hour
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 60.0 - 120 MPa8700 - 17400 psi
Back Pressure <= 4.00 MPa<= 580 psi
 
Descriptive Properties
Injection moldingYes
Injection speedslow
PelletsYes
Processing conditions acc. ISO9988-2
Profile extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kolon KOCETAL® UR304 Toughened Grade Acetal Resin
Celanese Celcon® GC90UV POM, 10% UV Resistant
Celanese Hostaform® C 9021 MD POM, 6% Stainless Steel Reinforced
Avient Lubri-Tech™ AT-000/5T Black Acetal-Copolymer, PTFE Lubricated
Avient LubriOne™ ATT-000/5T Black Acetal (POM) Copolymer

PHCQ145 / 178600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.