MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay ALKAMULS® OR 36 Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Ethoxylated castor oil. Emulsifier for oil and waxes in water based formulations. Used as dispersant for pigments and iron powders. Dispersant for pigments and iron powders in magnetic coupling fluids. Paper dye-leveling agent. Softening and rewetting agent for wet strength paper. Stabilizer for PVAc emulsion paints. Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 13.

Identification: ETHOXYLATED CASTOR OIL

CAS: 61791 – 12 – 6

Solubility: Soluble in water and most polar and aromatic solvents.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Emulsifier for Agrochemical formulations. Industrial formulations/Metal treatment : Emulsifier for oil and waxes in water based formulations. Used as dispersant for pigments and iron powders. Emulsifier for fats, oils, fatty acids, waxes and solvents. Dispersant for pigments and iron powders in magnetic coupling fluids. Paper dye-leveling agent. Softening and rewetting agent for wet strength paper. Stabilizer for PVAC emulsion paints. Emulsifier for Home and Personal Care formulations.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc
@Temperature 50.0 °C
0.0376 lb/in³
@Temperature 122 °F
pH 5.0 - 7.05.0 - 7.05% in water; RPG02
 
Thermal PropertiesMetricEnglishComments
Pour Point 12.0 °C53.6 °F
Flash Point >= 100 °C>= 212 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %Karl Fisher; RPG16
 
Descriptive Properties
AppearanceViscous Liquid
CompositionActive content1
HLB number13.1
Ionic ChargeNonionic
Saponification number60-69 mg KOH/gRPG05

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay ALKAMULS® VO/2003 Surfactant
Solvay ALKAMULS® OR 40 Surfactant
Solvay ALKAMULS® OR 10 Surfactant
Solvay GERONOL® TE 300 Surfactant
Solvay GERONOL® MS Surfactant

WRHOD044 / 137274

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.