MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sapco Si.SiC Silicon Carbide  (discontinued **)
Categories: Ceramic; Carbide

Material Notes: Information provided by Sapco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.10 g/cc0.112 lb/in³
Open Porosity 0.00 %0.00 %
Weibull Modulus 1010
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 9.09.0
Tensile Strength, Ultimate 390 MPa56600 psi
Modulus of Elasticity 410 GPa59500 ksi
Flexural Strength 400 MPa58000 psi
Compressive Strength 2000 MPa290000 psi
Poissons Ratio 0.240.24
Shear Modulus 165 GPa23900 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.30 µm/m-°C
@Temperature 20.0 °C
2.39 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°F
Thermal Conductivity 160 W/m-K1110 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1350 °C2460 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
Silicon Carbide, CVD
Silicon Nitride, reaction sintered
Ceradyne Ceralloy® 147-A Hot Pressed Silicon Nitride (Si3N4)
Sapco S.SiC Silicon Carbide

CSAP05 / 1967

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.