MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES Elastoblend® PA6/6 GF13 IM HS BK 13% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled; Nylon 66, Heat Stabilized; Nylon 66, Impact Grade

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight

Additive: Heat Stabilizer, Impact Modifier and Lubricant

Features: Heat Stabilized, Impact Modified and Lubricated

UL File Number: E157318

Appearance: Black

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.90 %
@Time 86400 sec
0.90 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.016 cm/cm
@Thickness 3.17 mm
0.016 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ASTM D785
Tensile Strength, Yield 82.7 MPa12000 psiASTM D638
Elongation at Break 6.0 %6.0 %ASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 36.2 GPa5250 ksiASTM D790
Izod Impact, Notched  1.07 J/cm
@Thickness 3.17 mm,
Temperature -40.0 °C
2.00 ft-lb/in
@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
 1.82 J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
3.40 ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 19.3 kV/mm490 kV/inMethod A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 79.2 µm/m-°C44.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 252 °C485 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 70G13HS1L BK031 PA66-GF13
Techmer ES HiFill FR® PA6 GF13 FR-N IM BK 13% Glass Filled
Akro-Plastic Akromid® A3 1 S3 black (1139) PA 66, Impact Resistant, Heat Stabilized, Conditioned
Celanese Nilit FRIANYL B63 HS-GV10 Nylon 6 for injection molding, 10% glass fiber reinforced
RTP Company RTP 2185 Polyetherimide (PEI); Carbon Fiber

PTPC1085 / 137023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.