MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Polystone® M Virgin UHMW-PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:
  • High abrasion and wear resistance
  • Low coefficient of friction
  • High impact strength
Product applications:
  • Food processing
  • Bulk material handling
  • Conveyor and packaging

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D792
Water Absorption <= 0.10 %<= 0.10 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62 - 6662 - 66ASTM D2240
Tensile Strength, Yield 21.4 MPa3100 psiASTM D638
Elongation at Break >= 350 %>= 350 %ASTM D638
Tensile Modulus 0.689 GPa100 ksiASTM D638
Flexural Strength 24.1 MPa3500 psiASTM D790
Compressive Strength 20.7 MPa3000 psiASTM D695
Izod Impact, Notched (ISO) 125 kJ/m²59.5 ft-lb/in²ASTM D4020
Coefficient of Friction, Dynamic 0.10 - 0.220.10 - 0.22Dry vs. Steel
Coefficient of Friction, Static 0.15 - 0.200.15 - 0.20Dry vs. Steel
Sand Slurry 100100
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D257
Surface Resistivity per Square <= 1.00e+12 ohm<= 1.00e+12 ohmASTM D257
Dielectric Constant 2.3
@Frequency 1e+6 Hz
2.3
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 45.0 kV/mm1140 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 198 µm/m-°C110 µin/in-°FASTM D696
Melting Point 130 - 135 °C266 - 275 °F
Maximum Service Temperature, Air 82.2 °C180 °F
Deflection Temperature at 1.8 MPa (264 psi) 42.2 °C108 °FASTM D648
Vicat Softening Point 82.2 °C180 °FISO 306
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF YesYes
USDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Okulen® 1000 PE-UHMW, Natural
Overview of materials for High Density Polyethylene (HDPE), Extruded
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Polikim ULPOLEN® 1000 UHMWPE Standard
Polikim ULPOLEN® 500 UHMWPE Standard

PROCH003 / 66207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.