MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aurora Plastics GPP6100-116C PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus and high impact.  It is designed for use in injection molded industrial power supply systems and to meet their stringent criterion. The superior balance of flow, allows the material to maintain excellent aesthetics over long flow lengths.  Available in a wide spectrum of colors.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 - 1.17 g/cc1.14 - 1.17 g/ccASTM D792
Melt Flow 16 - 20 g/10 min16 - 20 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 17.9 MPa>= 2600 psiASTM D638
Tensile Strength, Yield >= 26.2 MPa>= 3800 psiASTM D638
Elongation at Break >= 28 %>= 28 %ASTM D638
Flexural Modulus 2.24 GPa325 ksiTangent, Method B; ASTM D790
Izod Impact, Notched >= 0.320 J/cm>= 0.600 ft-lb/inASTM D256
 0.454 J/cm0.850 ft-lb/innominal; ASTM D256
Gardner Impact >= 12.6 J>= 9.30 ft-lbASTM D5420
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.9 kV/mm
@Thickness 3.40 mm
480 kV/in
@Thickness 0.134 in
Method A; ASTM D419
Dielectric Breakdown 64000 V64000 VASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) >= 107.4 °C>= 225.3 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.6 °C130 °FASTM D648
Vicat Softening Point 148.6 °C299.5 °FASTM D1525
Flammability Test 5.0
@Thickness 1.59 mm
5.0
@Thickness 0.0625 in
Oxygen Index >= 25 %>= 25 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastics Group Polifil® RMT-40V 40% Talc-Reinforced Polypropylene, High Impact, UV Stabilized
Plastics Group Polifil® RMC-40V 40% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized
LyondellBasell Moplen EP380S Polypropylene, Impact Modified; Molded/Extruded
LG Chemical LUPOL HF5254A PP+MF20%
Kraton® G1657 + PP blend + Talc (12/21/67)

PSEPO060 / 141023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.