MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aluminum Castings

Aluminum 242.0-T571, Sand Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 242.0-T571; UNS A02420; ISO 3522 and R164 AlCu4Ni2Mg2; AA242.0-T571; Al242.0-T571
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.81 g/cc0.102 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 70 - 10070 - 100AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 109109Estimated from Brinell Hardness.
Hardness, Rockwell A 3636Estimated from Brinell Hardness.
Hardness, Rockwell B 5353Estimated from Brinell Hardness.
Hardness, Vickers 9696Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 200 MPa>= 29000 psiAA
Tensile Strength, Yield 205 MPa
@Strain 0.2 %
29700 psi
@Strain 0.2 %
typical
Elongation at Break 0.50 %0.50 %in 50 mm
Tensile Modulus 71.0 GPa10300 ksiCompressive modulus in is typically about 2% higher for Al alloys
Compressive Yield Strength 235 MPa34100 psi
Poissons Ratio 0.330.33
Fatigue Strength 75.0 MPa
@# of Cycles 5.00e+8
10900 psi
@# of Cycles 5.00e+8
Notch Status unknown, R.R. Moore Test
Machinability 70 %70 %0-100 Scale (100=best)
Shear Modulus 26.5 GPa3840 ksi
Shear Strength 180 MPa26100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000510 ohm-cm0.00000510 ohm-cmAA; Typical 34% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lb
CTE, linear  22.7 µm/m-°C
@Temperature 20.0 - 100 °C
12.6 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical
 24.5 µm/m-°C
@Temperature 20.0 - 300 °C
13.6 µin/in-°F
@Temperature 68.0 - 572 °F
AA; Typical; average over range
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°F
Thermal Conductivity 134 W/m-K928 BTU-in/hr-ft²-°FAA; Typical at 25°C
Melting Point 532 - 635.0 °C990 - 1175 °FAA; Typical
Solidus 532 °C990 °FAA; Typical
Liquidus 635.0 °C1175 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Melt Temperature 677 - 816 °C1250 - 1500 °F
Solution Temperature 518 - 524 °C965 - 975 °F
Aging Temperature 168 - 174 °C335 - 345 °F40 - 48 hrs; No Solution heat treatment.
Casting Temperature 677 - 788 °C1250 - 1450 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 88.3 - 93.6 %88.3 - 93.6 %As remainder
Chromium, Cr <= 0.25 %<= 0.25 %
Copper, Cu 3.5 - 4.5 %3.5 - 4.5 %
Iron, Fe <= 1.0 %<= 1.0 %
Magnesium, Mg 1.2 - 1.8 %1.2 - 1.8 %
Manganese, Mn <= 0.35 %<= 0.35 %
Nickel, Ni 1.7 - 2.3 %1.7 - 2.3 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.70 %<= 0.70 %
Titanium, Ti <= 0.25 %<= 0.25 %
Zinc, Zn <= 0.35 %<= 0.35 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 242.0-T571, Permanent Mold Cast
Aluminum 242.0-T61, Sand Cast
Aluminum 242.0-T77, Sand Cast
Aluminum 242.0-O, Sand Cast
Aluminum 242.0-T21, Sand Cast

MAC2420T5S / 9810

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.