MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zinc Alloy 7; AG40B; Zn-4Al-0.015Mg; Zamak7
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Recommended Casting Temperature 395-425°C

Key Words: ASTM AG40B; UNS Z33522 (Ingot); UNS Z33523 (Castings); ZA-7; Zamak7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.60 g/cc0.238 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8080500 kg load; 10 mm hardened steel ball
Hardness, Knoop 9999Estimated from Brinell Value
Hardness, Vickers 8686Estimated from Brinell Value
Tensile Strength, Ultimate 285 MPa41300 psiUnspecified Heat Treatment
Tensile Strength, Yield 285 MPa
@Strain 0.2 %
41300 psi
@Strain 0.2 %
As Cast
Elongation at Break 14 %14 %As Cast; in 5 cm
Compressive Strength 414 MPa60000 psi
Fatigue Strength 47.0 MPa
@# of Cycles 5.00e+8
6820 psi
@# of Cycles 5.00e+8
Reverse Bend
Shear Strength 214 MPa31000 psi
Charpy Impact, Unnotched 58.0 J42.8 ft-lbAfter Aging 10 Years
 58.0 J
@Thickness 6.35 mm
42.8 ft-lb
@Thickness 0.250 in
square bar
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000640 ohm-cm0.00000640 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.4 µm/m-°C
@Temperature 20.0 °C
15.2 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.419 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 113 W/m-K784 BTU-in/hr-ft²-°F
Melting Point 381 - 387 °C718 - 729 °F
Solidus 381 °C718 °F
Liquidus 387 °C729 °F
 
Processing PropertiesMetricEnglishComments
Casting Temperature 395 - 425 °C743 - 797 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 3.5 - 4.3 %3.5 - 4.3 %Casting
 3.9 - 4.3 %3.9 - 4.3 %Ingot form
Cadmium, Cd <= 0.0020 %<= 0.0020 %Casting
 <= 0.0020 %<= 0.0020 %Ingot form
Copper, Cu <= 0.10 %<= 0.10 %Ingot form
 <= 0.25 %<= 0.25 %Casting
Iron, Fe <= 0.075 %<= 0.075 %Casting
 <= 0.075 %<= 0.075 %Ingot form
Lead, Pb <= 0.0020 %<= 0.0020 %Ingot form
 <= 0.0030 %<= 0.0030 %Casting
Magnesium, Mg 0.0050 - 0.020 %0.0050 - 0.020 %Casting
 0.010 - 0.020 %0.010 - 0.020 %Ingot form
Nickel, Ni 0.0050 - 0.020 %0.0050 - 0.020 %Casting
 0.0050 - 0.020 %0.0050 - 0.020 %Ingot form
Tin, Sn <= 0.0010 %<= 0.0010 %Casting
 <= 0.0010 %<= 0.0010 %Ingot form
Zinc, Zn 95.48 - 96.085 %95.48 - 96.085 %As balance; Ingot per ASTM B 240
 95.329 - 96.49 %95.329 - 96.49 %As balance; Castings per ASTM B 86

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc AC41A Alloy (Zamak 5), As Cast
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast
Zinc AC41A (Zamak 5), Cast and Aged
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast and Aged
Zinc AC43A (Zinc Alloy 2; Zn-4Al-2.5Cu-0.04Mg; Number 2 Die Casting Alloy; Zamak 2), Die Cast

MZN700 / 14541

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.