MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MetalTek MTEK CW-2M Cast UNS N26455 Severe Corrosion and Heat Resistant Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Information provided by MetalTek

Key Words: Cast UNS N26455; Cast Grade CW-2M; Cast ASTM A494; AMS 5408 (Centrifugal Casting); Wrought UNS N06455; Wrought Grade HASTELLOY® C4C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 495 MPa>= 71800 psi
Tensile Strength, Yield >= 275 MPa>= 39900 psi
Elongation at Break >= 20 %>= 20 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 15 - 17.5 %15 - 17.5 %
Iron, Fe <= 2.0 %<= 2.0 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 15 - 17.5 %15 - 17.5 %
Nickel, Ni 60.18 - 70 %60.18 - 70 %As Balance
Silicon, Si <= 0.80 %<= 0.80 %
Tungsten, W <= 1.0 %<= 1.0 %
 
Descriptive Properties
Heat TreatmentSol. Anneal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Nistelle C4C Nickel Superalloy
MetalTek MTEK CW-12MW Cast UNS N30002 Severe Corrosion and Heat Resistant Alloy
MetalTek MTEK N-7M Cast UNS N30007 Severe Corrosion and Heat Resistant Alloy
MetalTek MTEK CZ-100 Cast UNS N02100 Severe Corrosion and Heat Resistant Alloy
MetalTek MTEK CX-2MW Cast UNS N26022 Severe Corrosion and Heat Resistant Alloy

NMETEK126 / 18376

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.