MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Zytel® PLS FR95G15DH2 BK269 Nylon 6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: 15% Glass Reinforced Flame Retardant Heat Stabilized Polyamide

Zytel PLSFR95G15DH2 BK269 is 15% glass reinforced flame retardant black PA using SHIELD Technology only from DuPont exceptional resistance in hot air

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Key Words: PA-GF15FR(17)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inDAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inDAM; ISO 294-4 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 138 MPa20000 psiDAM; ISO 527-1/-2
Elongation at Break 2.6 %2.6 %DAM; ISO 527-1/-2
Tensile Modulus 7.35 GPa1070 ksiDAM; ISO 527-1/-2
Flexural Strength 197 MPa28600 psiDAM; ISO 178
Flexural Modulus 6.50 GPa943 ksiDAM; ISO 178
Charpy Impact Unnotched 3.90 J/cm²18.6 ft-lb/in²DAM; ISO 179/1eU
 3.60 J/cm²
@Temperature -30.0 °C
17.1 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 0.640 J/cm²3.05 ft-lb/in²DAM; ISO 179/1eA
 0.620 J/cm²
@Temperature -30.0 °C
2.95 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °C496 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 237 °C459 °FDAM; ISO 75-1/-2
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
DAM; IEC 60695-11-10
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
DAM; IEC 60695-11-10
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Part Marking Code>PA-GF15FR(17)<ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA-GF15FR(17)
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tritan™ MX710 Medical Grade Copolyester
Eastman Tritan™ MX711 Medical Grade Copolyester
Eastman Tritan™ MX730 Medical Grade Copolyester
Eastman Tritan™ MX731 Medical Grade Copolyester
Eastman Tritan™ MX810 Medical Grade Copolyester

PZDSY5472 / 161299

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.