MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C19500, H10 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability.

Applications: electrical springs, sockets, terminals, connectors, clips and other current carrying parts having strength.

Available as flat products.

Key Words: Strescon Copper, CDA 195
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.92 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B >= 90>= 90
Tensile Strength, Ultimate >= 670 MPa>= 97200 psi
Tensile Strength, Yield >= 650 MPa>= 94300 psi
Elongation at Break <= 2.0 %<= 2.0 %In 50 mm
Modulus of Elasticity 119 GPa17300 ksi
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000344 ohm-cm
@Temperature 20.0 °C
0.00000344 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.9 µm/m-°C
@Temperature 20.0 - 300 °C
9.39 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 199 W/m-K
@Temperature 20.0 °C
1380 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1085 - 1090 °C1985 - 1990 °F
Solidus 1085 °C1985 °F
Liquidus 1090 °C1990 °F
Annealing Point 399 - 593 °C750 - 1100 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.020 %<= 0.020 %
Cobalt, Co 0.60 - 1.0 %0.60 - 1.0 %
Copper, Cu 97 %97 %
Iron, Fe 1.3 - 1.7 %1.3 - 1.7 %
Lead, Pb <= 0.020 %<= 0.020 %
Other, total <= 0.10 %<= 0.10 %
Phosphorus, P 0.080 - 0.12 %0.080 - 0.12 %
Tin, Sn 0.40 - 0.70 %0.40 - 0.70 %
Zinc, Zn <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
High Strength Modified Copper, UNS C19400, O50 Temper flat products
High Strength Modified Copper, UNS C19400, O60 Temper flat products
Copper, UNS C19500, H02 Temper
Copper, UNS C19500, H08 Temper
Copper, UNS C19500, O61 Temper

MC19500b6 / 10966

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.