MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elkem (Bluestar Silicones) CAF® 530 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: CAF 530 is a one component silicone elastomer curing at Room Temperature as soon as the product comes into contact with atmospheric moisture:
  • Alcohol type, neutral
  • Non flowing, thixotropic
  • White, black and grey
  • Self-Adhesive (primer-less)
Applications: CAF 530 has been specially developed for professional customers. It is mainly attended as a flexible bonding and sealing agent between different types of materials substrate subject to thermal strain, as glass, metal or plastic with high thermal stability:
  • Maintenance and servicing in general industry.
  • Sealing & Bonding of metallic components.
  • Sealing & Bonding of plastic engineering components.
CAF 530 is specially used for applications where high performance primer-less adhesion and/or neutrality is required, such as:
  • Electrical & Electronic
  • Bonding of headlamps
  • Solar panels
Its chemical neutrality and bonding performances in hot and wet environment make CAF 530 the ideal protective product.Advantages: CAF 530 is a room temperature neutral cure elastomer used for applications which need neutrality guaranteeing no oxidation with metals principally used in electronic like copper.
  • Odourless, it is particularly well accepted in the workstation environment.
  • Outstanding adhesion on many substrates.
  • Good heat stability (-60°C to 185°C).
  • Good mechanical properties.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/cc
Storage Temperature 2.00 - 30.0 °C35.6 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3434ASTM D2240
Tensile Strength 1.20 MPa174 psiadhesion to Polycarbonate, ABS, PBT, Epoxy-PES, 1 mm thick, 14 days curing, norm NM750, 100% Cohesive failure
 1.20 MPa174 psiadhesion to Alu AG3, 1 mm thick, 14 days curing, norm NM748, 100% Cohesive failure
 1.30 MPa189 psiadhesion to PA 6.6, 30% fiber glass, 1 mm thick, 14 days curing, norm NM749, 100% Cohesive failure
 1.30 MPa189 psiadhesion to glass, 1 mm thick, 14 days curing, norm NM748, 100% Cohesive failure
 1.50 MPa218 psiadhesion to Stainless Steel/Glass, 1 mm thick, 14 days curing, norm NM748, 100% Cohesive failure
 3.50 MPa508 psiASTM D412
Elongation at Break 450 %450 %ASTM D412
100% Modulus 0.903 MPa
@Strain 100 %
131 psi
@Strain 100 %
ASTM D412
Adhesive Bond Strength 1.05 MPa152 psiPVF/PET, 90%, 100 h, 85°C, 85% RH
 1.08 MPa157 psiPVF, 90%, 100 h, 85°C, 85% RH
 1.10 MPa160 psiPVF/PET, 90%, Initial
 1.20 MPa174 psiPVF, 85%, Initial
Tear Strength 15.0 kN/m85.6 pliASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.90e+13 ohm-cm4.90e+13 ohm-cmIEC 60 093
Dielectric Constant 3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
IEC 60 250
Dielectric Strength 24.0 kV/mm610 kV/inIEC 60 243-1
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
IEC 60 250
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air  150 °C
@Time 3.60e+6 sec
302 °F
@Time 1000 hour
 185 °C
@Time 259000 sec
365 °F
@Time 72.0 hour
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Extrusion Rate 130 g/min130 g/min3mm, 3bars, norm 495A
Cure Time 10.0 - 15.0 min0.167 - 0.250 hourSkin formation
 480 min
@Thickness 2.00 mm
8.00 hour
@Thickness 0.0787 in
 1440 min
@Thickness 3.50 mm
24.0 hour
@Thickness 0.138 in
Tack-Free Time 40.0 min0.667 hour
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceNon flowing paste
ColorWhite, black & grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ V 1082 HiPro ST ~ PEX Silicone Rubber
Covestro Makrolon® AX 2677 Polycarbonate
Dow 3-4680 SILICONE GEL KIT
Dow 3120 RTV SILICONE RUBBER
Dow 1437 INDUSTRIAL SEALANT AND ADHESIVE

PBLUST094 / 191070

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.