MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Moplen HF501N Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Moplen HF501N is a non pelletized homopolymer powder. The product is non stabilized. When pelletized and activated Moplen HF501N is suitable for injection molding. The main applications for HF501N are mineral filled compounds, color and additives master batches, furniture. The properties reported below are measured on the pelletized and activated resin.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 50.0 MPa>= 7250 psiISO 527-1,-2
Tensile Strength, Yield 35.0 MPa5080 psiISO 527-1,-2
Elongation at Yield 9.0 %9.0 %ISO 527-1,-2
Tensile Modulus 1.55 GPa225 ksiISO 527-1,-2
Charpy Impact, Notched 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 155 °C311 °FISO 306
 
Descriptive Properties
Processing MethodCompounding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Moplen HP500N Polypropylene
BASF Novolen® 1125 N Polypropylene
BASF Novolen® 2600 M Polypropylene, Injection Molding Grade
BASF Novolen® 2500 H Polypropylene
BASF Novolen® 2300 L Polypropylene

PEQT8981 / 220615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.