MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Formosa Plastics Formolene® HB6007F High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Formolene® HB6007F is used for critical food packaging requirements. It has good stiffness properties and contains a antistatic additive to help dissipate dust particles on bottle surfaces. Formolene® HB6007F meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Suggested Applications: Milk Soft Drink Concentrate, Distilled Water Fruit Juice, etc.

Physical properties were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Condition E.

Information provided by Formosa Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.964 g/cc0.0348 lb/in³ASTM D1505
ESCR 100% Igepal® 15 - 20 hour15 - 20 hourCondition B, F50; ASTM D1693
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.3 MPa4400 psiASTM Type IV
Elongation at Break >= 300 %>= 300 %2 in/min, Type IV bar; ASTM D638
Flexural Modulus 1.65 GPa240 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -118 °C<= -180 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® HP4525 High Density Polyethylene
Formosa Plastics Formolene® HB5202B2 Sheet and Thermoforming HDPE
Formosa Plastics Formolene® E6210C High Density Polyethylene
Formosa Plastics Formolene® E6210A High Density Polyethylene
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene

PFPCPQ9002 / 239823

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.