MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total XLS 12 B High Density Polyethylene - Pipes and Fittings
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: HDPE XLS 12 B is a high performance hexene-based black compound, with a MRS 10 MPa - PE100 classification, primarily intended for extrusion of large diameter and thick wall pressure pipes.

Key characteristics are

  • a superior resistance to sagging, enabling the manufacture of very thick wall pipes with even wall distribution
  • an outstanding resistance to slow crack growth an rapid crack propagation ensuring safe and long-term network operation
  • an optimized formulation of additives and finely dispersed carbon black providing outstanding long-term stability in service

Designation ISO 1872-PE,E/M-ACGHL,50-T003

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.959 g/cc0.959 g/ccISO 1183
Carbon Black Loading 2.0 - 2.5 %2.0 - 2.5 %ISO 6964
Melt Flow 0.20 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.20 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133/T
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 220 °C374 - 428 °FExtrusion
 200 - 260 °C392 - 500 °FInjection
 
Descriptive Properties
Carbon Black Dispersion, Rating= 3ISO 18553
Thermal Stability 200°C> 20 minEN 728 / ISO 11357-6
Water Content= 300 ppmEN 12118, measured at the stage of compound manufacturing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total XT25N High Density Polyethylene, Pipe Resin
Total XSene® XRC 20 B High Density Polyethylene - Pipes and Fittings
TIMCAL ENSACO™ 150G Conductive Carbon Black
Borealis BorSafe™ HE3470-LS Black HDPE Compound for Pressure Pipes
Ineos K46-06-161 HDPE Copolymer with Carbon Black

PTOTAL730 / 130455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.