MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Estane® 54611 Polyester-Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Feature: Facilitates to produce high coating weight in one pass high production speed. Broad process window and transparent spherical pellets.

Uses: Melt roll coated fabrics and unsupported foils.

Available in Americas, Europe, Middle East, Africa and India

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccISO 2781
Maximum Moisture Content 0.100.10
Melt Flow 45 - 65 g/10 min
@Load 8.70 kg,
Temperature 190 °C
45 - 65 g/10 min
@Load 19.2 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ISO 868
Tensile Strength at Break 36.0 MPa5220 psiISO 527-3/5/500
Elongation at Break 670 %670 %
50% Modulus 4.30 MPa
@Strain 50 %
4.30 MPa
@Strain 50 %
100% Modulus 4.80 MPa
@Strain 100 %
696 psi
@Strain 100 %
300% Modulus 7.20 MPa
@Strain 300 %
1040 psi
@Strain 300 %
Tear Strength 49.0 kN/m280 pliISO 34B
Abrasion 4040[mm3]
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Zone 1 175 °C347 °FExtrusion
Zone 2 175 °C347 °FExtrusion
Zone 3 170 °C338 °FExtrusion
Zone 4 170 °C338 °FExtrusion
Adapter Temperature 165 °C329 °F5, Extrusion
Die Temperature 165 °C329 °F6, Extrusion
Roll Temperature 150 °C302 °F1, Extrusion
 160 °C320 °F2, Extrusion
Drying Temperature 90.0 °C194 °F
Dry Time 3.00 hour3.00 hour
Dew Point -40.0 - -30.0 °C-40.0 - -22.0 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane
Lubrizol Estane® 54601 Thermoplastic Polyurethane
Lubrizol ESTANE® 54620 Ester Based Thermoplastic Polyurethane

PNOVEON553 / 121444

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.