MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyMirae Clyrell EC340R Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Clyrell EC340R is a clarified polyolefinic resin designed for injection molding applications. Clyrell EC340R combines the aesthetic properties of a random with the impact-stiffness property of a heterophasic copolymer. Clyrell EC340R features is a high impact resistance at room and sub-zero temperature, good transparency and good resistance to stress whitening Clyrell EC340R can be used in clear impact container for food or non food applications, toys, housewares.

Product Features: high impact resistance at room and sub-zero temperature, good transparency and good resistance to stress whitening, and low shrinkage

Typical Applications: clear impact container for food or non food applications, toys, housewares.

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASMT D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.6 MPa3130 psiASTM D638
Flexural Modulus 0.932 GPa135 ksiASTM D790
Izod Impact, Notched  0.490 J/cm
@Temperature -20.0 °C
0.918 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 1.47 J/cm
@Temperature 23.0 °C
2.76 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen RP343N Injection Molding Grade Polypropylene
PolyMirae Clyrell EC340Q Injection Molding Grade Polypropylene
PolyMirae Moplen EP5015 Injection Molding Grade Polypropylene
PolyMirae Moplen EP500M Injection Molding Grade Polypropylene
PolyMirae Moplen RP340N Injection Molding Grade Polypropylene

PMIRAF10 / 183231

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.