MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® B3GM35 Q611 15/25% Glass/Mineral Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Ultramid B3GM35 Q611 is a 40% combined glass-fiber and mineral reinforced injection molding PA6 grade.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ISO 1183
Water Absorption 6.6 %6.6 %ISO 62
Moisture Absorption at Equilibrium 2.0 %2.0 %23°C/50% R.H.; ISO 62
Viscosity Number 130 cm³/g1.30 dl/g
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM Data; MD
Melt Flow 25 g/10 min
@Load 5.00 kg,
Temperature 275 °C
25 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 120 MPa17400 psi5mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5mm/min; ISO 527
Tensile Modulus 8.00 GPa1160 ksi1mm/min; ISO 527
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179
 5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor  0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
 0.020
@Frequency 100 Hz
0.020
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 400 V400 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 38.0 µm/m-°C21.1 µin/in-°FISO 11359
Melting Point 220 °C428 °F10 K/min
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0626 in
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 3216 PBT, 15% Glass Reinforced
Polyplastics Duranex® 3216 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 15% GF filled
BASF Ultramid® B3GM35 Q643 15/25% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)

PBASF9313 / 85077

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.