MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Daplen™ EE002AE Polypropylene Elastomer Modified
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties and gives a good surface quality. Applications: automotive exterior applications including bumpers and exterior trims.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Linear Mold Shrinkage 0.0015 cm/cm0.0015 in/inpost shrinkage (2h/90°C)
 0.014 cm/cm0.014 in/inmold average
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
11 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ISO 868
Ball Indentation Hardness 36.0 MPa5220 psi132N/10s; ISO 2039
Tensile Strength, Yield 19.0 MPa2760 psi50mm/min; ISO 527-2
Elongation at Break >= 150 %>= 150 %50mm/min; ISO 527-2
Elongation at Yield 5.5 %5.5 %50mm/min; ISO 527-2
Tensile Modulus 0.950 GPa138 ksi1mm/min; ISO 527-2
Flexural Strength 21.0 MPa3050 psiISO 178
Flexural Modulus 0.900 GPa131 ksi2mm/min; ISO 178
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -20.0 °C
5.71 ft-lb/in²
@Temperature -4.00 °F
ISO 180/1A
 57.0 kJ/m²
@Temperature 23.0 °C
27.1 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.850 J/cm²
@Temperature -20.0 °C
4.04 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C
@Temperature -30.0 - 80.0 °C
55.6 µin/in-°F
@Temperature -22.0 - 176 °F
Borealis Method
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °FISO 75-2
Vicat Softening Point  45.0 °C
@Load 5.10 kg
113 °F
@Load 11.2 lb
ISO 306
 135 °C
@Load 1.02 kg
275 °F
@Load 2.25 lb
ISO 306
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 - 80.0 °C104 - 176 °F
Melt Temperature 220 - 260 °C428 - 500 °Fmass temperature
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Injection Velocity 100 - 200 mm/sec3.94 - 7.87 in/sec
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
 
Descriptive Properties
Back Pressurelow to medium
Screw Speedlow to medium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Daplen™ ED117AE Polypropylene TPO Compound
Borealis Bormed™ RF830MO Polypropylene Copolymer for Healthcare Applications
Borealis Daplen™ EE115AE TPO Compound
Borealis Daplen™ EE040AE TPO Compound
Borealis Daplen™ ED135AI TPO Compound

PBOREA405 / 108664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.