MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI KYDEX® T Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: High impact fire-rated sheet

KYDEX® T is a proprietary thermoplastic sheet that is cost competitive with fire retardant ABS/PVC (FR-ABS) formulations but with significantly higher impact strength and extensibility

KYDEX® T is less hygroscopic, unlike FR-ABS, it typically does not require pre-drying, offers superior impact, more uniform forming with less wall thinning and offers significantly greater resistance to a broad range of corrosive chemicals and cleaning solutions. It is available in a wide range of aesthetic choices and is Underwriter's Laboratories, Inc® recognized Std 94 V-0, 5V.

Suggested Applications:

  • Aircraft Interiors
  • Equipment Housings
  • Kiosk Housings
  • Mass Transit Vehicle Interior Components
  • Medical Products

Features:

  • Substitute for FR-ABS sheet with competitive pricing but superior cost/performance
  • Higher breakage resistance measured by the Notched Izod test than competitive thermoplastics
  • Available in thicknesses from 0.71 mm (0.028 in) and up, in eight textures, a variety of colors, custom blank sizes and low minimums
  • Among the most rigid of thermoforming materials with a modulus of elasticity of 2,482 MPa (360,000 psi)
  • Easy to form with excellent part definition and deep-draw characteristics
  • Recognized by Underwriter's Laboratories, Inc® for Std 94 V-0, 5V in all thicknesses
  • Form times similar to FR-ABS making it an easy transition from competitive products

Values based upon 3.18 mm (0.125 in) sheet unless otherwise specified

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9494ASTM D785
Tensile Strength 42.0 MPa6090 psiASTM D638
Elongation at Break 110 %110 %ASTM D638
Modulus of Elasticity 2.48 GPa360 ksiASTM D790
Flexural Strength 66.0 MPa9570 psiASTM D790
Izod Impact, Notched 8.01 J/cm
@Temperature 22.8 °C
15.0 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 75.6 °C168 °FAnnealed; ASTM D648
Flammability, UL94 V-0V-0UL File E115252; Component Recognition
 5VB
@Thickness >=0.711 mm
5VB
@Thickness >=0.0280 in
Underwriters Laboratories, Inc®, File E115252; Component Recognition; UL Standard 94
 
Descriptive Properties
FlammabilityPassFAR 25.853(a)(i); Vertical Burn, 60 sec
 PassFAR 25.853(a)(ii); Vertical Burn, 12 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® 100 Polymer Alloy Sheet
SEKISUI SPI KYDEX® T-LW Thermoplastic
SEKISUI SPI KYDEX® 510 Thermoplastic
SEKISUI SPI KYDEX® 6565 Thermoplastic
SEKISUI SPI KYDEX® 410 ABS/PVC

PSEKIS046 / 185871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.