MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric  (discontinued **)
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3K

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  745 MPa
@Temperature -55.0 °C
108000 psi
@Temperature -67.0 °F
Dry
 855 MPa
@Temperature 24.0 °C
124000 psi
@Temperature 75.2 °F
Dry
 855 MPa
@Temperature 71.0 °C
124000 psi
@Temperature 160 °F
Dry
Tensile Modulus  62.7 GPa
@Temperature 71.0 °C
9090 ksi
@Temperature 160 °F
Dry
 63.4 GPa
@Temperature 24.0 °C
9200 ksi
@Temperature 75.2 °F
Dry
 64.8 GPa
@Temperature -55.0 °C
9400 ksi
@Temperature -67.0 °F
Dry
Flexural Yield Strength 276 MPa40000 psiLong Beam, dry
Compressive Yield Strength  400 MPa
@Temperature 71.0 °C
58000 psi
@Temperature 160 °F
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 655 MPa
@Temperature 24.0 °C
95000 psi
@Temperature 75.2 °F
Dry
Compressive Modulus  59.3 GPa
@Temperature 71.0 °C
8600 ksi
@Temperature 160 °F
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 64.1 GPa
@Temperature 24.0 °C
9300 ksi
@Temperature 75.2 °F
Dry
Bearing Yield Strength 848 MPa
@Temperature 24.0 °C
123000 psi
@Temperature 75.2 °F
Dry
Shear Strength  26.2 MPa
@Temperature 71.0 °C
3800 psi
@Temperature 160 °F
Short Beam, Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 60.0 MPa
@Temperature 24.0 °C
8700 psi
@Temperature 75.2 °F
Short Beam, Jet Fuel (30 ± 1 days of Jet A Fuel (ASTM D1655) at 75 ± 5°F (24 ± 3°C)
 61.0 MPa
@Temperature 24.0 °C
8850 psi
@Temperature 75.2 °F
Short Beam, Dry
 61.4 MPa
@Temperature 24.0 °C
8910 psi
@Temperature 75.2 °F
Short Beam, Skydrol (30 ± 1 days of Type 2 Skydrol Hydraulic Fluid at 140 ± 5°F (60 ± 3°C)
 
Descriptive Properties
Dry Resin Content (%)37-41Prepreg
Flow (%)8-20
Wet Resin Content (%)52Laminate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Thornel® P-75 Carbon Fiber/Epoxy Advanced Composite System
Solvay Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System
Solvay LTM® 26EL Epoxy with T300 Woven Carbon Fiber Laminate
Hexcel® HexPly® 8552 Epoxy Matrix, Carbon Fabric Form
Overview of materials for Epoxy/Carbon Fiber Composite

PHEXC142 / 98612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.