MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Elvaloy® 741WR Ethylene/Vinyl Acetate/Carbon Monoxide (E/VA/CO) Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: DuPont™ Elvaloy® 741WR an ethylene/vinyl acetate/carbon monoxide (E/VA/CO) copolymer. The difference between Elvaloy®741 and Elvaloy®741WR, is that Elvaloy®741WR contains a wax additive to deter pellet blocking in packaging/distribution/handling.

DuPont™ ELVALOY® 741WR Resin Modifier complies with Food and Drug Administration Regulation 21 CFR 175.105 - - Adhesives. This Regulation describes adhesives that may be used as components of articles intended for use in packaging, transporting, or holding food, subject to the limitations and requirements therein.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ASTM D792, ISO 1183
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
35 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength 5.90 MPa856 psiASTM D638
Elongation at Break 950 %950 %ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 66.0 °C151 °FASTM D3418, ISO 3146
Glass Transition Temp, Tg -32.0 °C-25.6 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 240 °C<= 464 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvaloy® AC 1330 Ethylene Methyl Acrylate
Dow Elvaloy® AC 2618 Ethylene Methyl Acrylate
Mateck Highly Oriented Pyrolytic Graphite
Dow Elvaloy® AC 12024S Ethylene Methyl Acrylate
Dow Elvaloy® HP662 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer

PDTA4936 / 170376

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.