MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micro-organisms, such as algae, bacteria and fungi. The antimicrobial effect remains during the entire life time of the product. POM CG-plastics are often used in medical and food products and facilities due additional protection.

Information provided by CENTROPLAST Engineering Plastics GMBH

Key Words: POM CG
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Moisture Absorption 0.200 %
@Temperature 23.0 °C
0.200 %
@Temperature 73.4 °F
normal humidity; ISO 62
Water Absorption at Saturation 0.80 %
@Temperature 23.0 °C
0.80 %
@Temperature 73.4 °F
ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8484test piece 10mm thick; ISO 2039-2
Ball Indentation Hardness 140 MPa20300 psiISO 2039-1
Tensile Strength 63.0 MPa9140 psi5 mm/min; ISO 527-2
Tensile Strength, Yield 63.0 MPa9140 psi50 mm/min; ISO 527-2
Elongation at Break 31 %31 %ISO 527-2
Tensile Modulus 2.60 GPa377 ksiISO 527-2
Flexural Modulus 2.50 GPa363 ksiISO 178
Charpy Impact Unnotched 22.0 J/cm²105 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/IeA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 60250
 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inin transformer oil; IEC 60243-1
Dissipation Factor  0.0030
@Frequency 100 Hz
0.0030
@Frequency 100 Hz
IEC 60250
 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C
@Temperature 23.0 - 60.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359
Thermal Conductivity 0.310 W/m-K2.15 BTU-in/hr-ft²-°FDIN 52612
Melting Point 165 °C329 °FDSC, 10 K/m; ISO 3146
Maximum Service Temperature, Air 105 °C221 °Fcontinuous
 140 °C284 °Fshort term
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C205 °FISO 75-2
Vicat Softening Point 150 °C302 °FVST/B/50; ISO 306
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 HB
@Thickness 3.00 - 6.00 mm
HB
@Thickness 0.118 - 0.236 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood Compliance
 
Descriptive Properties
ColorNatural
Food Compliance BfR:Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Americhem Engineered Compounds ColorRx™ ABS-0505ARX Biocompatible, Antimicrobial ABS
Americhem Engineered Compounds ColorRx™ ABS-0502ARX Biocompatible, Antimicrobial ABS
Americhem Engineered Compounds ColorRx™ ABS-0501A Antimicrobial ABS
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures
Celanese Celcon® MT12U03 Medical Grade Acetal Copolymer

PCENTR50 / 150229

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.