MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

INEOS Styrolution Lustran® 348 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Lustran® 348 resin is an injection molding grade of ABS (Acrylonitrile butadiene styrene) with medium-impact and high-gloss. Healthcare certifications, High gloss, Medium impact, Meets FDA modified ISO 10993-1 requirements, Meets U.S. Pharmacopeia 23 Class VI test requirements. Applications: Components of intravenous (IV)systems, Surgical instruments, Diagnostic test kits

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D 955
Melt Flow  5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D 1238
 14 g/10 min
@Load 10.0 kg,
Temperature 220 °C
14 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 112112ASTM D 785
Tensile Strength, Yield 48.3 MPa7010 psiASTM D 638
Tensile Modulus 2.62 GPa380 ksiASTM D 638
Flexural Strength 75.8 MPa11000 psiASTM D 790
Flexural Modulus 2.69 GPa390 ksiASTM D 790
Izod Impact, Notched 2.14 J/cm
@Temperature 23.0 °C
4.00 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 81.0 µm/m-°C45.0 µin/in-°FASTM D 696
Deflection Temperature at 0.46 MPa (66 psi) 92.7 °C199 °Funannealed; ASTM D 648
 100 °C212 °Fannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C186 °Funannealed; ASTM D 648
 95.6 °C204 °Fannealed; ASTM D 648
Vicat Softening Point 107 °C
@Load 1.02 kg
225 °F
@Load 2.25 lb
B/2 120C/H; ASTM D 1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 246 - 274 °C475 - 525 °F
Mold Temperature 29.0 - 60.0 °C84.2 - 140 °F
Drying Temperature 79.0 °C
@Time 7200 - 14400 sec
174 °F
@Time 2.00 - 4.00 hour
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® ST801 NC010A PA66-HI
Covestro Bayblend® T80 XG PC/ABS Blend
Polykemi AB POLYblend 65H MA5 PC/ABS-blend, Low Friction
RTP Company RTP 300 TFE 5 Polycarbonate (PC), PTFE Lubricated
Samyang Triloy® 215 PC/ABS alloy

PSTYR9850 / 216077

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.