MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Stratasys® RGD525 High Temperature Material
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes:

Information provided by Stratasys

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 - 1.18 g/cc1.17 - 1.18 g/ccPolymerized; ASTM D792
Water Absorption 1.2 - 1.4 %
@Time 86400 sec
1.2 - 1.4 %
@Time 24.0 hour
ASTM D570-98
Ash 0.38 - 0.42 %0.38 - 0.42 %USP281
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 78 - 8378 - 83
Hardness, Shore D 87 - 8887 - 88
Tensile Strength at Break 70.0 - 80.0 MPa10200 - 11600 psiASTM D638-03
Elongation at Break 10 - 15 %10 - 15 %ASTM D638-03
Modulus of Elasticity 3.20 - 3.50 GPa464 - 508 ksiASTM D638-04
Flexural Strength 110 - 130 MPa16000 - 18900 psiASTM D790-03
Flexural Modulus 3.10 - 3.50 GPa450 - 508 ksiASTM D790-04
Izod Impact, Notched 0.140 - 0.160 J/cm0.262 - 0.300 ft-lb/inASTM D256-06
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 63.0 - 67.0 °C145 - 153 °FASTM D648-06
 75.0 - 80.0 °C167 - 176 °Fafter thermal post treatment procedure A; ASTM D648-06
Deflection Temperature at 1.8 MPa (264 psi) 55.0 - 57.0 °C131 - 135 °FASTM D648-07
Glass Transition Temp, Tg 62.0 - 65.0 °C144 - 149 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Stratasys® ABS-M30
Proto3000 Objet RGD525 High Temperature Prototyping Polymer
Stratasys® Ultem 9085 for Rapid Prototyping
Stratasys® FDM Nylon 12™ 3D Printing Polymer; Conditioned
Markforged Onyx 3D Printed Nylon Carbon Composite

PSTRAT246 / 206343

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.