MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Plansee Ta2.5W Tantalum-Tungsten 2.5 Alloy
Categories: Metal; Nonferrous Metal; Refractory Metal

Material Notes: Tantalum-Tungsten alloys possess good mechanical properties and excellent corrosion resistance. Ta2.5W is stronger than pure tantalum, yet it remains easy to work at high temperatures, up to 1 600 °C. Common applications for Ta2.5W are as heat exchangers and heating elements used in the chemical equipment construction field.

Information provided by Plansee.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 16.67 g/cc16.67 g/cccalculated
 
Component Elements PropertiesMetricEnglishComments
Tantalum, Ta 98.5 %98.5 %
Tungsten, W 2.5 %2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tantalum, Ta; Annealed
Mi-Tech Metals HD17 Tungsten-Based Metal
Plansee Ta10W Tantalum-Tungsten 10 Alloy
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
Goodfellow Tantalum 90/Tungsten 10 Alloy

NPLAM955 / 135511

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.