MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Isoflon PA 12 Polyamide 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes:
  • General use for mechanical parts
  • Good heat resistance
  • Easy to use

Information provided by Isoflon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccDIN 53479
Water Absorption 0.80 %0.80 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D785
Tensile Strength 44.0 MPa6380 psiDIN 53455
Elongation at Break 150 %150 %DIN 53455
Tensile Modulus 1.55 GPa225 ksiDIN 53457
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmDIN 53482
Dielectric Constant 3.5
@Frequency 1000 Hz
3.5
@Frequency 1000 Hz
DIN 53483
Dielectric Strength 20.0 - 30.0 kV/mm508 - 762 kV/inDIN 53481
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C61.1 µin/in-°FDIN 52328
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FDIN 52612
Melting Point 185 °C365 °FDIN 53736
Maximum Service Temperature, Air 80.0 °C176 °FContinuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C129 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °FContinuous; DIN 52612
 
Descriptive Properties
ColorNat.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hippe PA 12 Nylon 12
Overview of materials for Nylon 12
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Evonik VESTAMID® NRG 3001 PA 12
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer

PISOFL914 / 123302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.