MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 20%Glass Fiber Filled

Material Notes:

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 - 0.800 g/cc0.0253 - 0.0289 lb/in³
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Water Absorption 1.6 %1.6 %ISO 62
Moisture Absorption at Equilibrium 0.60 %0.60 %23°C; 50% RH; ISO 62
Viscosity Test 56 cm³/g0.56 dl/gISO 307
Linear Mold Shrinkage, Flow 0.0036 cm/cm0.0036 in/inISO 2577, 294-4
Linear Mold Shrinkage, Transverse 0.0061 cm/cm0.0061 in/inISO 2577, 294-4
Melt Flow 43.5 g/10 min
@Load 10.0 kg,
Temperature 360 °C
43.5 g/10 min
@Load 22.0 lb,
Temperature 680 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 205 MPa
@Load 98.0 kg,
Time 30.0 sec
29700 psi
@Load 216 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength at Break 125 MPa18100 psiISO 527-1/-2
Elongation at Break 2.5 %2.5 %ISO 527-1/-2
Tensile Modulus 7.30 GPa1060 ksiISO 527-1/-2
Izod Impact, Notched (ISO) 6.50 kJ/m²3.09 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 4.70 J/cm²22.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 75-1/-2
 23.0 µm/m-°C
@Temperature 180 °C
12.8 µin/in-°F
@Temperature 356 °F
DIN 53752
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75-1/-2
Glass Transition Temp, Tg 225 °C437 °FISO 11357-1/-2
Decomposition Temperature >= 400 °C>= 752 °F
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Ignition Temperature 580 - 600 °C1080 - 1110 °FDIN 54836
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper throat
Zone 1 350 °C662 °FFeed zone
Zone 2 360 °C680 °FCompression
Zone 3 370 °C698 °FMetering-zone
Zone 4 370 °C698 °FNozzle
Melt Temperature 350 - 390 °C662 - 734 °FInjection molding/extrusion
 370 °C698 °FOptimal
Mold Temperature 150 - 190 °C302 - 374 °FInjection molding
 170 °C338 °FOptimal
Drying Temperature 140 °C284 °F
Dry Time 4 hour4 hour
 
Descriptive Properties
Commercial StatusEurope
Primary Processing TechniqueInjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® E 1010 PES
BASF Ultrason® E 6020 P PES
BASF Ultrason® S 3010 MR UN PSU
CENTROPLAST CENTRO HPM Polysulfone
BASF Ultrason® S 2010 PSU

PBASG0173 / 131806

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.