MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon® M6138 High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Applications
ALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness. Typical applications include agricultural bins, crates, trays and consumer durable goods.

Regulatory Status
M 6138 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing M 6138 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.961 g/cc0.0347 lb/in³ASTM D1505
Melt Flow 3.8 g/10 min3.8 g/10 minASTM D1238
Spiral Flow 20.8 cm8.20 inSpiral channel (0.625” insert) with injection pressure of 1000 psi at 440°F.; Equistar
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6969ASTM D2240
Tensile Strength at Break 26.5 MPa3850 psiCrosshead speed - 2"min.; ASTM D638
Tensile Strength, Yield 30.8 MPa4460 psiCrosshead speed - 2"min.; ASTM D638
Elongation at Yield 7.7 %7.7 %ASTM D638
Flexural Modulus, 1% Secant 1520 MPa220000 psiCrosshead speed - 0.5" min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C169 °FASTM D648
Vicat Softening Point 126 °C259 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 °C450 °F
Middle Barrel Temperature 232 °C450 °F
Front Barrel Temperature 232 °C450 °F
Nozzle Temperature 246 °C475 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil HD 6040.UV High Density Polyethylene Resin
Borealis MG7547S Polyethylene
Borealis Bormed™ HE7541-PH HDPE for Healthcare Applications
LyondellBasell Alathon® M6060 High Density Polyethylene
Mocom (ALBIS) ALTECH® PE-HD A 2040/500 GF40 HDPE

PEQU0434 / 36877

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.