MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® 20NSP Nylon 66, General Purpose
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Vydyne 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin with a further enhanced crystallization temperature. Designed to crystallize rapidly in order to reduce cycle times and increase productivity through faster part set-up.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DAM; ISO 1183
Water Absorption 1.64 %
@Time 86400 sec
1.64 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 2.4 %2.4 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm
@Thickness 2.00 mm
0.013 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.017 cm/cm
@Thickness 2.00 mm
0.017 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 64.0 MPa9280 psi50% RH; ISO 527-2
 90.0 MPa13100 psiDAM; ISO 527-2
Tensile Strength, Yield 67.0 MPa9720 psi50% RH; ISO 527-2
 95.0 MPa13800 psiDAM; ISO 527-2
Elongation at Break 15 %15 %DAM; ISO 527-2
 23 %23 %50% RH; ISO 527-2
Elongation at Yield 5.2 %5.2 %DAM; ISO 527-2
 18 %18 %50% RH; ISO 527-2
Tensile Modulus 2.30 GPa334 ksi50% RH; ISO 527-2
 3.40 GPa493 ksiDAM; ISO 527-2
Flexural Strength 28.0 MPa4060 psi50% RH; ISO 178
 103 MPa14900 psiDAM; ISO 178
Flexural Modulus 1.20 GPa174 ksi50% RH; ISO 178
 3.30 GPa479 ksiDAM; ISO 178
Poissons Ratio 0.400.40ISO 527-2
Izod Impact, Notched (ISO)  3.00 kJ/m²
@Temperature -40.0 °C
1.43 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 3.00 kJ/m²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 4.00 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 4.00 kJ/m²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -40.0 °C
1.43 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.300 J/cm²
@Temperature -40.0 °C
1.43 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm
@Thickness 1.00 mm
1.00e+13 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
Arc Resistance 120 - 180 sec
@Thickness 3.00 mm
120 - 180 sec
@Thickness 0.118 in
PLC 5; ASTM D 495
Hot Wire Ignition, HWI 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 15 - 30 sec15 - 30 secPLC 3; UL 746
 30 - 60 sec30 - 60 secPLC 2; UL 746
High Amp Arc Ignition, HAI 60 - 120 arcs60 - 120 arcsPLC 1; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min0.000 - 0.394 in/minUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
55.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 262 °C504 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 221 °C430 °FUnannealed; 50% RH; ISO 75-2/B
 232 °C450 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical  130 °C
@Thickness 0.400 mm
266 °F
@Thickness 0.0157 in
UL 746
 130 °C
@Thickness 0.710 mm
266 °F
@Thickness 0.0280 in
UL 746
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  75.0 °C
@Thickness 0.400 mm
167 °F
@Thickness 0.0157 in
UL 746
 75.0 °C
@Thickness 0.710 mm
167 °F
@Thickness 0.0280 in
UL 746
 75.0 °C
@Thickness 1.50 mm
167 °F
@Thickness 0.0591 in
UL 746
 75.0 °C
@Thickness 3.00 mm
167 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  75.0 °C
@Thickness 0.400 mm
167 °F
@Thickness 0.0157 in
UL 746
 85.0 °C
@Thickness 0.710 mm
185 °F
@Thickness 0.0280 in
UL 746
 85.0 °C
@Thickness 1.50 mm
185 °F
@Thickness 0.0591 in
UL 746
 85.0 °C
@Thickness 3.00 mm
185 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-2
@Thickness 0.400 mm
V-2
@Thickness 0.0157 in
 V-2
@Thickness 0.710 mm
V-2
@Thickness 0.0280 in
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
Oxygen Index 26 %26 %DAM; EN ISO 4589-2
Glow Wire Ignition Temperature  825 °C
@Thickness 0.400 mm
1520 °F
@Thickness 0.0157 in
IEC 60695-2-13
 850 °C
@Thickness 0.710 mm
1560 °F
@Thickness 0.0280 in
IEC 60695-2-13
 850 °C
@Thickness 1.50 mm
1560 °F
@Thickness 0.0591 in
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-12
 960 °C
@Thickness 0.710 mm
1760 °F
@Thickness 0.0280 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 280 °C500 - 536 °FInjection
Middle Barrel Temperature 270 - 285 °C518 - 545 °FInjection
Front Barrel Temperature 280 - 290 °C536 - 554 °FInjection
Nozzle Temperature 280 - 300 °C536 - 572 °FInjection
Melt Temperature 285 - 300 °C545 - 572 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AdditiveLubricant
Agency RatingsASTM, D4066 PA0131
 ASTM, D6779 PA0131
 EC, 1935/2004
 EU, 10/2011
 EU, 2023/2006
 FDA, 21 CFR 177.1500
 FED, L-P-410A
 NSF, STD-51
AppearanceNatural Color
Automotive Material SpecificationToyota TSM5516G Class 2 (compliance)
FeaturesFast Molding Cycle
 General Purpose
 Good Mold Release
 Good Stiffness
 High Crystallinity
 High Rigidity
 Lubricated
 Nucleated
FormsPellets
Outdoor Suitabilityf2UL 746C
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, General Purpose
Ascend Performance Materials Vydyne® 21SPC Nylon 66, General Purpose
Arkema Rilsan® BESVO A FDA Nylon 11
CENTROPLAST CENTROMID 6.6 FG Polyamide 6.6, Food Grade
Akro-Plastic Akromid® A3 GF 30 1 black PA 6.6 Dry, 30% Glass Filled, Heat Stabilized

PASCE9738 / 220841

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.