MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 1006 Steel, cold drawn
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: The composition listed is for standard grade for wire and rod.

Applications: Soft, very ductile, used in applications which require severe bending and welding such as panels for automobiles or appliances. Also used in magnet core applications.

Key Words: UNS G10060, ASME 5041, ASTM A29, ASTM A510, ASTM A545, FED QQ-W-461, MIL SPEC MIL-S-11310 (CS1006), SAE J403, SAE J412, SAE J414, AISI1006
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.872 g/cc0.2844 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 9595
Hardness, Knoop 113113Converted from Brinell
Hardness, Rockwell B 5555Converted from Brinell
Hardness, Vickers 9898Converted from Brinell
Tensile Strength, Ultimate 330 MPa47900 psi
Tensile Strength, Yield 285 MPa41300 psi
Elongation at Break 20 %20 %In 50 mm
Reduction of Area 45 %45 %
Modulus of Elasticity 206 GPa29900 ksi
Bulk Modulus 163 GPa23600 ksiEstimated from elastic modulus
Poissons Ratio 0.290.29Typical for steel
Machinability 50 %50 %Based on AISI 1212 steel = 100%. Group I bar, rod, and wire products machinability can be improved by cold drawing.
Shear Modulus 80.0 GPa11600 ksiEstimated from elastic modulus
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000174 ohm-cm0.0000174 ohm-cmTypical steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.6 µm/m-°C
@Temperature 0.000 - 100 °C
7.00 µin/in-°F
@Temperature 32.0 - 212 °F
 13.5 µm/m-°C
@Temperature 0.000 - 300 °C
7.50 µin/in-°F
@Temperature 32.0 - 572 °F
 13.7 µm/m-°C
@Temperature 0.000 - 1000 °C
7.61 µin/in-°F
@Temperature 32.0 - 1830 °F
 14.2 µm/m-°C
@Temperature 0.000 - 500 °C
7.89 µin/in-°F
@Temperature 32.0 - 932 °F
Specific Heat Capacity 0.481 J/g-°C0.115 BTU/lb-°F50-100ºC
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Iron, Fe 99.43 - 99.75 %99.43 - 99.75 %As remainder
Manganese, Mn 0.25 - 0.40 %0.25 - 0.40 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1005 Steel
AISI 1010 Steel, cold drawn
AISI 1006 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round
AISI 1006 Steel, CQ, DQ, and DQSK sheet, 1.6-5.8 (0.06-0.23 in) mm thick
AISI 1008 Steel, CQ, DQ, and DQSK sheet, 1.6-5.8 mm thick

M1006A / 6774

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.