MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Diorite
Categories: Ceramic

Material Notes: Igneous rock, with a grain size 1- 3 mm (hypabyssal). It is intermediate in the acidic-basic range, with a total silica content of 55-65%. Predominant minerals in this generally medium-dark colored rock are hornblende and plagioclase feldspar.

Property values are typical of Diorite used in construction. Actual property values will vary from sample to sample.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.70 - 3.03 g/cc0.0975 - 0.109 lb/in³
Porosity 0.30 - 2.7 %0.30 - 2.7 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore H 40 - 9240 - 92
Hardness, Mohs 4.76 - 6.214.76 - 6.21
Tensile Strength, Ultimate 15.0 - 30.0 MPa2180 - 4350 psi
Modulus of Elasticity 70.0 - 100 GPa10200 - 14500 ksi
Modulus of Rupture 0.0138 - 0.0552 GPa2.00 - 8.01 ksi
Compressive Strength 124 - 303 MPa18000 - 44000 psi
Impact Toughness 2.20 - 13.4 cm/cm²5.60 - 34.0 in/in²
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.00 - 3.00 µm/m-°C
@Temperature 20.0 °C
1.11 - 1.67 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.669 - 0.808 J/g-°C0.160 - 0.193 BTU/lb-°F
Thermal Conductivity 2.30 W/m-K16.0 BTU-in/hr-ft²-°F

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Basalt
Limestone
Granite
Cordierite, 2MgO-2Al2O3-5SiO2
Andesite

BMIN028 / 187

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.