MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MarkeTech Rutile (TiO2) Fiber Optic Crystal  (discontinued **)
Categories: Ceramic; Oxide; Titanium Oxide

Material Notes: More chemically and physically resistant than Yttrium Vanadate. Large birefringence. Used for fiber optic beam displacers and optical isolators. Grown by Vernull method. Transmission range 500 to 4500 nm.

Data provided by MarkeTech International. MarkeTech International is no longer in business.

Key Words: TiO2; Titanium Dioxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.26 g/cc0.154 lb/in³
a Lattice Constant 4.5936 Å4.5936 Å
c Lattice Constant 2.9852 Å2.9852 Å
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 7.07.0
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  160
@Frequency 1e+7 Hz
160
@Frequency 1e+7 Hz
 200
@Frequency 10000 Hz
200
@Frequency 10000 Hz
Band Gap 3.3 eV3.3 eV
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.14 µm/m-°C3.97 µin/in-°Fa direction
 9.19 µm/m-°C5.11 µin/in-°Fc direction
Thermal Conductivity 9.00 W/m-K62.5 BTU-in/hr-ft²-°Fa direction
 13.0 W/m-K90.2 BTU-in/hr-ft²-°Fc direction
Melting Point 1840 °C3340 °F
Debye Temperature 487 °C909 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 2.472.47η o
 2.732.73η e
Transmission, Visible 90 %
@Wavelength >=500 nm
90 %
@Wavelength >=500 nm
transparent range; thickness not reported
 
Descriptive Properties
Crystal StructureTetragonal

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Dioxide, Brookite
Titanium Dioxide, Rutile
Titanium Dioxide, TiO2, Anatase
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
CeramTec 192/193 Titania

C5MT831 / 120740

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.