MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
Filler Content 35 %35 %Mineral Filler
Linear Mold Shrinkage, Flow 0.014 - 0.022 cm/cm0.014 - 0.022 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 53.8 MPa7800 psiASTM D638
Elongation at Break 24 %24 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 3.47 GPa503 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 93.1 MPa13500 psiASTM D790
Flexural Modulus 2.81 GPa408 ksiASTM D790
Izod Impact, Notched 0.590 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
1.11 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
@Thickness 3.18 mm
163 °F
@Thickness 0.125 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 277 - 299 °C531 - 570 °F
Mold Temperature 82.2 - 104 °C180 - 219 °F
Drying Temperature 71.1 - 82.2 °C160 - 180 °F
Dry Time 2.00 hour2.00 hour
 
Descriptive Properties
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAutomotive Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® R AR 218 V30 Nylon 66, 30% glass fiber, DRY
Domo TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY
Celanese Zytel® 70G35EF BK538 PA66-GF35
Envalior Durethan® DP AKV 35 LT H2.0 904040 Nylon 66, 35% Glass Fiber
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized

PH0POL1271 / 145840

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.