MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polycasa AKRYLON XT PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT sheets also combine the following excellent properties: brilliant transparency, very good weathering and ageing resistance, high surface stability/resistance, and good recyclability.

Construction components

  • Light domes
  • Partition walls
  • Glazing
  • Roofing
  • Windows for caravans

Lighting

  • Prismatic control lenses
  • Opal diffusers

Engineering components

  • Housings
  • Machine Covers

Advertising and Decorations

  • Letters
  • Decorations
  • Shop fittings
  • Advertising panels
  • Point of Purchase Displays

Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 175 MPa25400 psiISO 2039-1
Tensile Strength at Break 70.0 MPa10200 psiISO 527-2
Elongation at Break 4.0 %4.0 %ISO 527-2
Tensile Modulus 3.20 GPa464 ksiISO 527-2
Flexural Strength 115 MPa16700 psiISO 178
Charpy Impact Unnotched 1.70 J/cm²8.09 ft-lb/in²ISO 179
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 - 5.00e+15 ohm-cm1.00e+15 - 5.00e+15 ohm-cmIEC 60093
Surface Resistance 3.00e+15 - 3.00e+16 ohm3.00e+15 - 3.00e+16 ohmIEC 60093
Dielectric Constant  2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
 2.7
@Frequency 50 Hz
2.7
@Frequency 50 Hz
 3.1
@Frequency 1000 Hz
3.1
@Frequency 1000 Hz
Dielectric Strength 30.0 kV/mm
@Thickness 1.00 mm
762 kV/in
@Thickness 0.0394 in
DIN 53481
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
DIN 53752
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75
Vicat Softening Point 105 °C221 °FISO 306
Decomposition Temperature >= 280 °C>= 536 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4921.492ISO 489
Haze 0.60 %0.60 %AKRYLON XT clear; ISO 14782
Transmission, Visible 93 %
@Thickness 3.00 mm
93 %
@Thickness 0.118 in
ISO 1183
 
Descriptive Properties
Combustibility GradeEEN 13501-1
Electrical Strength, kV/mm²10IEC 60243-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 899 X 131271 A Acetal (POM), High Purity - Wear Resistant
Polycasa Vision CAST PMMA
Spartech Polycast SP 1.25 Cell Cast Acrylic
Akzo Nobel Expancel® 461 DE 20 d70 Dry expanded microspheres
Trinseo Plexiglas® V825 Acrylic

PSF0231 / 66582

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.