MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SSAB Tunnplat Aluzink F26A Metal-coated Mild Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: Metal-coated Mild Steel

Comments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manufacturer.

Data provided by SSAB Tunnplat.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Estimated by MatWeb
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate <= 420 MPa<= 60900 psi
Tensile Strength, Yield <= 300 MPa
@Strain 0.2 %,
Thickness <=0.700 mm
<= 43500 psi
@Strain 0.2 %,
Thickness <=0.0276 in
20 MPa higher apply
Elongation at Break >= 26 %>= 26 %A80; For thicknesses < 0.70 mm values 2% lower apply
Bend Radius, Minimum >= 1.0 t>= 1.0 t90° bending; avoid bending and rebending
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 98 %98 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SSAB Tunnplat Aluzink B500A Metal-coated Mild Steel
SSAB Tunnplat Dogal B420 Metal-coated Mild Steel
SSAB Tunnplat Dogal B500 Metal-coated Mild Steel
SSAB Tunnplat Dogal F26 Metal-coated Mild Steel
SSAB Tunnplat Aluzink B420A Metal-coated Mild Steel

NTUNN61 / 19553

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.