MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

China Tungsten YG8 Tungsten Carbide for Dies and Wear Part Making
Categories: Ceramic; Carbide

Material Notes: For drawing and straightening steels, non-ferrous metal and alloy bars and tubings; and for fabricating of machine parts, tools and wear parts, such as nozzles centres, guiding devices, upsetting dies and perforating tools

Information provided by China Tungsten

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 14.5 - 14.9 g/cc0.524 - 0.538 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A >= 89>= 89
Flexural Strength 1470 MPa213000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
China Tungsten YG8 Tungsten Carbide for Cutting Tools
China Tungsten YG8 Tungsten Carbide
China Tungsten YG8 Cemented Tungsten Carbide for Mining Purposes
H.C. Starck AmperitĀ® 512.074 Agglomerated Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12
AISI Type H13 Hot Work Tool Steel

NCHIN089 / 78931

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.