MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BNZ Materials Bazelite 2000 Insulating Castable
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for installation by various methods including gunning, casting or slap-troweling. Each product is specifically formulated to economically obtain the desired properties for the application and service temperature for which it is intended.

Information provided by BNZ Materials Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0370 lb/in³Fired at 5 hrs at 816°C
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.000460 GPa
@Temperature 540 °C
0.0667 ksi
@Temperature 1000 °F
Fired; ASTM C258
 0.000620 GPa
@Temperature 815 °C
0.0899 ksi
@Temperature 1500 °F
ASTM C258
 0.000620 GPa
@Temperature 1095 °C
0.0899 ksi
@Temperature 2003 °F
ASTM C258
 0.00103 GPa
@Temperature 104 °C
0.149 ksi
@Temperature 219 °F
Dried; ASTM C258
Compressive Strength  2.34 MPa
@Temperature 1095 °C
340 psi
@Temperature 2003 °F
 2.90 MPa
@Temperature 815 °C
420 psi
@Temperature 1500 °F
 2.96 MPa
@Treatment Temp. 540 °C
430 psi
@Treatment Temp. 1000 °F
Cold Crush Strength; Fired at 540°C
 4.14 MPa
@Treatment Temp. 104 °C
600 psi
@Treatment Temp. 219 °F
Cold Crush Strength; Dried 104°C
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1149 °C2100 °F
Shrinkage  0.10 %
@Temperature 540 °C
0.10 %
@Temperature 1000 °F
Permanent Linear Change; ASTM C210
 0.20 %
@Temperature 815 °C
0.20 %
@Temperature 1500 °F
Permanent Linear Change; ASTM C210
 0.30 %
@Temperature 1095 °C
0.30 %
@Temperature 2003 °F
Permanent Linear Change; ASTM C210
 
Component Elements PropertiesMetricEnglishComments
Al2O3 34 %34 %
CaO 15.8 %15.8 %
Fe2O3 6.5 %6.5 %
MgO 0.30 %0.30 %
Na2O 0.80 %0.80 %Includes K2O
SiO2 40.1 %40.1 %
TiO2 1.9 %1.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gromax PBT 4115-104D 15% Glass Fiber Filled
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled
Meehanite HSV Heat Resisting Cast Iron
COI Ceramics Nextel™ AS-N610 Oxide Ceramic Matrix Composite, Aluminosilicate
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate

CBNZ941 / 149181

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.