MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 47.9 %47.9 %Laminate Fiber Volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  253 MPa
@Temperature 177 °C
36700 psi
@Temperature 351 °F
Wet
 259 MPa
@Temperature 132 °C
37600 psi
@Temperature 270 °F
Wet
 281 MPa
@Temperature 177 °C
40800 psi
@Temperature 351 °F
Dry
 349 MPa
@Temperature 132 °C
50600 psi
@Temperature 270 °F
Dry
 392 MPa
@Temperature -54.0 °C
56900 psi
@Temperature -65.2 °F
Dry
 399 MPa
@Temperature 24.0 °C
57900 psi
@Temperature 75.2 °F
Wet
 428 MPa
@Temperature 24.0 °C
62100 psi
@Temperature 75.2 °F
Dry
Tensile Modulus  20.2 GPa
@Temperature 177 °C
2930 ksi
@Temperature 351 °F
Wet
 21.8 GPa
@Temperature 177 °C
3160 ksi
@Temperature 351 °F
Dry
 24.5 GPa
@Temperature 132 °C
3550 ksi
@Temperature 270 °F
Wet
 24.7 GPa
@Temperature 132 °C
3580 ksi
@Temperature 270 °F
Dry
 25.1 GPa
@Temperature 24.0 °C
3640 ksi
@Temperature 75.2 °F
Wet
 25.2 GPa
@Temperature -54.0 °C
3660 ksi
@Temperature -65.2 °F
Dry
 26.5 GPa
@Temperature 24.0 °C
3840 ksi
@Temperature 75.2 °F
Dry
Compressive Yield Strength  52.0 MPa
@Temperature 177 °C
7540 psi
@Temperature 351 °F
Wet
 71.0 MPa
@Temperature 132 °C
10300 psi
@Temperature 270 °F
Wet
 85.0 MPa
@Temperature 177 °C
12300 psi
@Temperature 351 °F
Dry
 104 MPa
@Temperature 132 °C
15100 psi
@Temperature 270 °F
Dry
 128 MPa
@Temperature 24.0 °C
18600 psi
@Temperature 75.2 °F
Wet
 199 MPa
@Temperature -54.0 °C
28900 psi
@Temperature -65.2 °F
Dry
 308 MPa
@Temperature 24.0 °C
44700 psi
@Temperature 75.2 °F
Dry
Compressive Modulus  12.1 GPa
@Temperature 177 °C
1750 ksi
@Temperature 351 °F
Wet
 15.2 GPa
@Temperature 132 °C
2200 ksi
@Temperature 270 °F
Wet
 15.6 GPa
@Temperature 177 °C
2260 ksi
@Temperature 351 °F
Dry
 17.2 GPa
@Temperature 132 °C
2490 ksi
@Temperature 270 °F
Dry
 19.7 GPa
@Temperature 24.0 °C
2860 ksi
@Temperature 75.2 °F
Wet
 24.8 GPa
@Temperature -54.0 °C
3600 ksi
@Temperature -65.2 °F
Dry
 28.1 GPa
@Temperature 24.0 °C
4080 ksi
@Temperature 75.2 °F
Dry
Shear Strength  11.0 MPa
@Temperature 177 °C
1600 psi
@Temperature 351 °F
Short Beam
 14.0 MPa
@Temperature 177 °C
2030 psi
@Temperature 351 °F
Short Beam
 17.0 MPa
@Temperature 132 °C
2470 psi
@Temperature 270 °F
Short Beam
 23.0 MPa
@Temperature 132 °C
3340 psi
@Temperature 270 °F
Short Beam
 29.0 MPa
@Temperature -54.0 °C
4210 psi
@Temperature -65.2 °F
Short Beam
 30.0 MPa
@Temperature 24.0 °C
4350 psi
@Temperature 75.2 °F
Short Beam
 30.0 MPa
@Temperature 24.0 °C
4350 psi
@Temperature 75.2 °F
Short Beam
 
Descriptive Properties
Cured Thickness per Ply (cm)0.025Laminate
Dry Resin Content (%)47-53Prepreg
Flow (%)20-30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Hexcel® HexPly® F155 Epoxy Resin, K120 Kevlar Fabric
Hexcel® HexPly® F185 Epoxy Resin, 120 Glass Fabric
Hexcel® F161 Epoxy Resin, 120 Glass Fabric
Hexcel® HexForce™ 345 Aramid Fabric

PHEXC112 / 98582

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.