MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cadi 150 Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: A small addition of Zr to copper improves resistance to softening and resists deformation at high temperatures where normal copper would soften rapidly. Zirconium copper is used as a Class 1 electrode material to minimize sticking when resistance spot welding galvanized materials.

Forms:

  • Rod
  • Bar

Information provided by Cadi Company.

Key Words: UNS C15000
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B  55
@Diameter 50.8 - 76.2 mm
55
@Diameter 2.00 - 3.00 in
 60
@Diameter 25.4 - 50.8 mm
60
@Diameter 1.00 - 2.00 in
 >= 65
@Diameter <=25.4 mm
>= 65
@Diameter <=1.00 in
hard temper
Tensile Strength at Break  >= 345 MPa
@Thickness >=25.4 mm
>= 50000 psi
@Thickness >=1.00 in
 >= 414 MPa
@Thickness <=25.4 mm
>= 60000 psi
@Thickness <=1.00 in
Tensile Strength, Yield  >= 345 MPa
@Strain 0.5 %,
Thickness >=25.4 mm
>= 50000 psi
@Strain 0.5 %,
Thickness >=1.00 in
 >= 414 MPa
@Strain 0.5 %,
Thickness <=25.4 mm
>= 60000 psi
@Strain 0.5 %,
Thickness <=1.00 in
Modulus of Elasticity 117 GPa17000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.00000216 ohm-cm<= 0.00000216 ohm-cm>80% IACS, up to 3" diameter/any thickness
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 366.6 W/m-K2544 BTU-in/hr-ft²-°F
Melting Point 980.0 - 1080 °C1796 - 1976 °F
Solidus 980.0 °C1796 °F
Liquidus 1080 °C1976 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 649 °C1200 °FBrazing, <15 minutes
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 99.85 %99.85 %
Zirconium, Zr 0.15 %0.15 %
 
Descriptive Properties
RMWA Class1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 13 mm wire
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 2.3 mm wire, no aging
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 25 mm rod
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 6 mm rod
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 6 mm wire

NCADI02 / 15510

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.