MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

FKuR Kunststoff Fibrolon® P 8540 Wood-Plastic Compound, Fiber Reinforced
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Wood and Natural Products

Material Notes: FIBROLON® are fiber reinforced compounds. Fibrolon® P 8540 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-Composites: WPC), which, unlike many other WPC, can be injection molded without problems. Furthermore it is possible to process FIBROLON® to complex profiles, panels and hollow profiles and/or into components for the automotive interiors. FIBROLON® compounds are distinguished by high strength and a stiffness comparable to wood.

Information Provided by FKuR Kunststoff GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.360 g/cc0.0130 lb/in³ISO 60
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Melt Flow 2.0 - 3.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
2.0 - 3.0 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 24.0 MPa3480 psiISO 527
Tensile Strength, Yield 26.0 MPa3770 psiISO 527
Elongation at Break 4.5 %4.5 %ISO 527
Elongation at Yield 3.0 %3.0 %ISO 527
Tensile Modulus 3.40 GPa493 ksiISO 527
Flexural Yield Strength 41.0 MPa5950 psiat 3.5% strain; ISO 178
Flexural Modulus 3.50 GPa508 ksiISO 178
Charpy Impact Unnotched 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eU
Charpy Impact, Notched 0.360 J/cm²
@Temperature 23.0 °C
1.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 180 °C320 - 356 °FISO 3146-C
Vicat Softening Point 155 °C311 °FA; ISO 306
 
Descriptive Properties
Melt Volume Flow (cm3/10 min)3-4ISO 1133; 190°C, 5kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced
FKuR Kunststoff Fibronlon® P 8540 Wood-Plastic Composite
FKuR Kunststoff Fibronlon® S 7530 Wood-Plastic Composite
FKuR Kunststoff Biograde® C 6530 Biodegradable Plastic Compound

PFKUR011 / 107049

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.