MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo Plexiglas® Diffuse™ V045-68207 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: Plexiglas® Diffuse™ V045-68207 is a thermoplastic acrylic resin formulated for injection molding and extrusion applications in the LED lighting market. It is characterized by an excellent balance of transmission and hiding performance. It exhibits a textured surface when extruded.

Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Water Absorption 0.3 %0.3 %24 hr. immersion; ASTM D570
Linear Mold Shrinkage 0.002 - 0.006 cm/cm0.002 - 0.006 in/inASTM D955
Melt Flow 2.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8888ASTM D785
Tensile Strength, Ultimate 68.9 MPa10000 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Tensile Modulus 3.31 GPa480 ksiASTM D638
Flexural Strength 103 MPa15000 psiASTM D790
Flexural Modulus 3.00 GPa435 ksiASTM D790
Izod Impact, Notched 0.374 J/cm0.700 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C214 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 97.2 °C207 °Fannealed; ASTM D648
Vicat Softening Point 100 °C212 °F50°C/hr; 50N; ASTM D1525
 106 °C222 °F50°C/hr; 10N; ASTM D1525
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Haze >= 100 %
@Thickness 2.03 mm
>= 100 %
@Thickness 0.0800 in
ASTM D1003
Transmission, Visible 89 %
@Thickness 2.03 mm
89 %
@Thickness 0.0800 in
ASTM D1003
 
Descriptive Properties
ASTM ClassificationPMMA 0131T1V1ASTM D788

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Plexiglas® VS-UVT Acrylic
Trinseo Solarkote™ A200 Acrylic
Overview of materials for Acrylic, Optical Sheet
Overview of materials for Acrylic, Heat Resistant, Molded
Trinseo Plexiglas® V920 Acrylic

PARKG043l / 191488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.