MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.

Features: Outstanding flame retardant properties, especially suited for tray cables.

Uses: Cable jacket and hose and tube and injection molding and fabric coating

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 95
@Time 5.00 sec
95
@Time 0.00139 hour
ASTM D2240
Tensile Strength  10.3 MPa
@Temperature 121 °C,
Time 605000 sec
1500 psi
@Temperature 250 °F,
Time 168 hour
Air Oven
 11.7 MPa
@Temperature 113 °C,
Time 605000 sec
1700 psi
@Temperature 235 °F,
Time 168 hour
Air Oven
 13.8 MPa
@Temperature 100 °C,
Time 605000 sec
2000 psi
@Temperature 212 °F,
Time 168 hour
IRM 902 Oil
Tensile Strength, Ultimate 13.8 MPa2000 psiASTM D412
Elongation at Break 360 %360 %ASTM D412
 270 %
@Treatment Temp. 121 °C,
Time 605000 sec
270 %
@Treatment Temp. 250 °F,
Time 168 hour
Air Oven
 288 %
@Treatment Temp. 100 °C,
Time 605000 sec
288 %
@Treatment Temp. 212 °F,
Time 168 hour
IRM 902 Oil
 324 %
@Treatment Temp. 113 °C,
Time 605000 sec
324 %
@Treatment Temp. 235 °F,
Time 168 hour
Air Oven
100% Modulus 9.60 MPa
@Strain 100 %
1390 psi
@Strain 100 %
ASTM D412
300% Modulus 12.4 MPa
@Strain 300 %
1800 psi
@Strain 300 %
ASTM D412
Tear Strength 15.8 kN/m90.0 pliTrouser; ASTM D470
Graves Tear Strength 59.6 kN/m340 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 300
@Load 1.00 kg
300
@Load 2.20 lb
H-18 wheel; ASTM D3389
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.60e+12 ohm-cm5.60e+12 ohm-cmASTM D257
Surface Resistivity per Square 5.60e+14 ohm5.60e+14 ohmASTM D257
Dielectric Constant  4.5
@Frequency 1000 Hz
4.5
@Frequency 1000 Hz
ASTM D2520
 5.7
@Frequency 1e+6 Hz
5.7
@Frequency 1e+6 Hz
ASTM D2520
Dissipation Factor  0.040
@Frequency 1000 Hz
0.040
@Frequency 1000 Hz
ASTM D2520
 0.050
@Frequency 1e+6 Hz
0.050
@Frequency 1e+6 Hz
ASTM D2520
 
Thermal PropertiesMetricEnglishComments
Melting Point 175 °C347 °FDSC
Glass Transition Temp, Tg -30.0 °C-22.0 °FDSC
Flammability, UL94 V-0
@Thickness 0.762 mm
V-0
@Thickness 0.0300 in
Vertical Flame Test; ASTM D3801
Oxygen Index 38 %38 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 160 °C320 °FExtrusion
Zone 2 165 °C329 °FExtrusion
Zone 3 170 °C338 °FExtrusion
Zone 4 175 °C347 °FExtrusion
Adapter Temperature 180 °C356 °F5, Extrusion
Die Temperature 180 °C356 °F6, Zone 1, Extrusion
 180 °C356 °FZone 2, Extrusion
Drying Temperature 82.0 °C180 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 95 P 5003 TPU-Polyether
SPS Guang Zhou POFLEX™ EP8300 Cable Grade TPU
AlphaGary Garathane™ X 94-350 B Polyurethane based compound
Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane
Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant

PNOVEON600 / 121491

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.