MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Lupolen 2421K Low Density Polyethylene (LDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Lupolen 2421 K is an additivated, low density polyethylene. It is characterized by a good processability. Films made from Lupolen 2421 K exhibit good optical properties. It contains an antioxidant and is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications: Food Packaging Film, Hygiene Film, Shrink Film, Surface Protection Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ISO 1183-1
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 11.0 MPa1600 psiISO 527-1,-2
Film Elongation at Break, MD 300 %300 %ISO 527-1,-3
Film Elongation at Break, TD 600 %600 %ISO 527-1,-3
Tensile Modulus 0.260 GPa37.7 ksiISO 527-1,-2
Coefficient of Friction >= 0.70>= 0.70ISO 8295
Dart Drop Test 100 g0.221 lbF50; ASTM D 1709
Film Tensile Strength at Break, MD 22.0 MPa3190 psiISO 527-1,-3
Film Tensile Strength at Break, TD 17.0 MPa2470 psiISO 527-1,-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 111 °C232 °Fpeak; ISO 3146
Vicat Softening Point 92.0 °C198 °FA50N; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 8.0 %
@Thickness 0.0500 mm
<= 8.0 %
@Thickness 0.00197 in
ASTM D1003
Gloss >= 60 %>= 60 %@ 20°; ASTM D2457
 >= 105 %>= 105 %@ 60°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 190 °C302 - 374 °Fblown film extrusion
 
Descriptive Properties
Failure Energy (J/mm)3.5DIN 53373
Processing MethodBlown Film, Cast Film
Test Specimenfilm, 50µm blown film extruded at 170°C, and a blow up ratio 2.5:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman PE1059 Film Extrusion Polyethylene
Huntsman PE5050 Extrusion Coating Polyethylene
ExxonMobil LD 6520.BA Low Density Polyethylene Resin
Huntsman PE5030 Extrusion Coating Polyethylene
Westlake EC472 Low Density Polyethylene

PEQT8536 / 220171

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.