MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil C6LL 1017.63 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: ExxonMobil™ C6LL 1017.63 is an ethylene 1-hexene linear low density polyethylene resin formulated for blown film extrusion. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excellent drawability, make this a very versatile packaging film resin.

Availability: Latin America and North America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Freezer Film
  • Heavy Duty Bags
  • Ice Bags
  • Stretch Film
  • Trash Bags

Information provided by ExxonMobil

Key Words: LLDPE LL 3001.63
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ExxonMobil method
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 40.0 N9.00 lb (f)
Film Tensile Strength at Yield, MD 8.96 MPa1300 psiASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa1400 psiASTM D882
Film Elongation at Break, MD 540 %540 %ASTM D882
Film Elongation at Break, TD 790 %790 %ASTM D882
Puncture Energy 3.05 J2.25 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 310 g310 gASTM D1922
Elmendorf Tear Strength TD 710 g710 gASTM D1922
Dart Drop Test 170 g0.375 lbASTM D1709A
Film Tensile Strength at Break, MD 57.9 MPa8400 psiASTM D882
Film Tensile Strength at Break, TD 48.3 MPa7000 psiASTM D882
1% Secant Modulus, MD 193 MPa28000 psiASTM D882
1% Secant Modulus, TD 241 MPa35000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 124 °C<= 255 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 13 %13 %ASTM D1003
Gloss 38 %38 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force9 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LD 317.87 Film Resin
ExxonMobil HD 5805 High Density Polyethylene Resin
ExxonMobil Exceed™ 1318CA Blown Film Resin
ExxonMobil C6LL 1017.32 Cast Linear Low Density Polyethylene Resin
Chevron Phillips Marlex® HHM TR-130 MDPE Film Resin

PEX99157 / 175393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.