MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Special Metals INCOLOY® Alloy 909
Categories: Metal; Superalloy; Iron Base

Material Notes: A nickel-iron-cobalt alloy with a silicon addition and containing niobium and titanium for precipitation hardening. It is similar to INCOLOY alloys 903 and 907 in that it has low thermal expansion and high strength. However, the silicon addition results in improved notch-rupture and tensile properties that are achieved with less-restrictive processing and significantly shorter heat treatments. Used for gas-turbine casings, shrouds, vanes, and shafts. Standard product forms are round, flats, forging stock, extruded section, sheet, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: UNS N19909
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.30 g/cc0.300 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  1160 MPa
@Temperature 550 °C
168000 psi
@Temperature 1020 °F
Precipitation Hardened prior to test
 1300 MPa
@Temperature 23.0 °C
189000 psi
@Temperature 73.4 °F
Tensile Strength, Yield 1140 MPa
@Strain 0.2 %
165000 psi
@Strain 0.2 %
Precipitation Hardened. Value at room temperature
 950 MPa
@Strain 0.2 %,
Temperature 550 °C
138000 psi
@Strain 0.2 %,
Temperature 1020 °F
Precipitation Hardened prior to test
Elongation at Break 15 %15 %Precipitation Hardened
 15 %
@Temperature 550 °C
15 %
@Temperature 1020 °F
Precipitation Hardened prior to test.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000728 ohm-cm0.0000728 ohm-cm
Curie Temperature 400 - 455 °C752 - 851 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.70 µm/m-°C
@Temperature 20.0 - 427 °C
4.28 µin/in-°F
@Temperature 68.0 - 801 °F
Specific Heat Capacity 0.427 J/g-°C0.102 BTU/lb-°F
Thermal Conductivity 14.8 W/m-K103 BTU-in/hr-ft²-°F
Melting Point 1395 - 1430 °C2543 - 2610 °F
Solidus 1395 °C2543 °F
Liquidus 1430 °C2610 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.030 %0.030 %
Carbon, C 0.010 %0.010 %
Cobalt, Co 13 %13 %
Iron, Fe 42 %42 %
Nickel, Ni 38 %38 %
Niobium, Nb (Columbium, Cb) 4.7 %4.7 %
Silicon, Si 0.40 %0.40 %
Titanium, Ti 1.5 %1.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCOLOY® Alloy 907
Special Metals INCOLOY® Alloy 903
Special Metals NI-SPAN-C® Alloy 902
Waspaloy A Nickel Superalloy (UNS N07001)
Special Metals INCONEL® Alloy 718

NINC86 / 17429

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.