MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo MAGNUM™ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: MAGNUM™ 3904 is a medium heat ABS. Its very high impact properties make it suitable for main interior automotive applications. MAGNUM ™ 3904 is available in Europe and China, locally produced in major car production regions. Due to its excellent extrusion capabilities, this product is also used for large thermoformed parts, for Truck and Bus applications.

Benefits:

  • Lot to lot consistency allowing for optimal machine parameters setting from the start
  • Self-coloring enabling improvement of costs by using less pigments and lowering your logistic costs
  • Low VOC allowing a better interior air quality facing increasing regulatory and OEMs constraints
  • Heat stability during wide range of processing temperatures: enhanced part design freedom
  • Contains low amounts of gel providing for excellent thermoformability with low levels of scrap
Applications:
  • Main interior automotive applications requiring high impact
  • Various interior trims, under the beltline
  • Large sized applications in commercial transportation
Automotive Specifications:
  • BMW GS 93016
  • GM QK 002022 Color: Natural
  • DAIMLER DBL 5404.03
  • VAG VW-TL 527

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183/B
Apparent Bulk Density 0.650 g/cc0.0235 lb/in³ISO 60
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow 4.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.5 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  37.0 MPa
@Thickness 3.20 mm
5370 psi
@Thickness 0.126 in
Injection Molded; ISO 527-2/50
 39.0 MPa
@Thickness 3.20 mm
5660 psi
@Thickness 0.126 in
Injection Molded; ISO 527-2/100
Elongation at Yield  2.6 %
@Thickness 3.20 mm
2.6 %
@Thickness 0.126 in
Injection Molded; ISO 527-2/50
 2.8 %
@Thickness 3.20 mm
2.8 %
@Thickness 0.126 in
Injection Molded; ISO 527-2/100
Tensile Modulus 1.82 GPa
@Thickness 3.20 mm
264 ksi
@Thickness 0.126 in
Injection Molded; ISO 527-2
Flexural Strength 58.0 MPa
@Thickness 3.20 mm
8410 psi
@Thickness 0.126 in
2.0 mm/min, 3-points, Injection Molded; ISO 178
Flexural Modulus 1.90 GPa276 ksi2.0 mm/min, 3-points, Injection Molded; ISO 178
Izod Impact, Notched (ISO)  17.0 kJ/m²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
Injection Molded; ISO 180/A
 42.0 kJ/m²
@Temperature 23.0 °C
20.0 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 180/A
Charpy Impact, Notched  1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
Injection Molded; ISO 179/2C
 1.80 J/cm²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
Injection Molded; ISO 179/1eA
 2.20 J/cm²
@Temperature 23.0 °C
10.5 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179/2C
 3.70 J/cm²
@Temperature 23.0 °C
17.6 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C207 °FAnnealed; ISO 75-2/A
Vicat Softening Point 97.0 °C207 °FISO 306/B50
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Descriptive Properties
Carbon Emission20 µg/gVDA 277

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo MAGNUM™ 3904 Ultra Smooth ABS
Celanese Celanex® 2300 GV1/10 PBT, 10% Glass Reinforced
Trinseo MAGNUM™ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin
Trinseo Magnum™ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin
Celanese Celanex® 3316 PBT, 30% Glass Reinforced

PDWST070 / 142279

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.