MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® AKV 50 H2.0 901510 Nylon 66 (PA66), 50% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: PA 66, 50% glass fibers, injection molding, heat-aging stabilized

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³ISO 60
Density 1.57 g/cc0.0567 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.4 %1.4 %50% RH; ISO 62
Water Absorption at Saturation 4.0 %4.0 %ISO 62
Linear Mold Shrinkage, Flow 0.0023 cm/cm0.0023 in/in150x105x3; 300 °C / MT 80 °C; 400 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/in150x105x3; 300 °C / MT 80 °C; 400 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance  1050 N
@Temperature -30.0 °C
236 lb (f)
@Temperature -22.0 °F
ISO 6603-2
 1162 N
@Temperature 23.0 °C
261.2 lb (f)
@Temperature 73.4 °F
ISO 6603-2
Ball Indentation Hardness 246 MPa35700 psiISO 2093-1
Tensile Strength at Break 230 MPa33400 psi5 mm/min; ISO 527-1,-2
Elongation at Break 2.6 %2.6 %5 mm/min; ISO 527-1,-2
Tensile Modulus 16.0 GPa2320 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 260 MPa37700 psi2 mm/min; ISO 178-A
Flexural Modulus 14.0 GPa2030 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 3.0 %3.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 15.0 kJ/m²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  85.0 kJ/m²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
 85.0 kJ/m²
@Temperature -30.0 °C
40.4 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
Charpy Impact Unnotched  9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched  1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
Puncture Energy  2.80 J
@Temperature -30.0 °C
2.07 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 3.60 J
@Temperature 23.0 °C
2.66 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
 4.5
@Frequency 100 Hz
4.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm
@Thickness 1.00 mm
1020 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0090
@Frequency 100 Hz
0.0090
@Frequency 100 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 V550 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 261 °C502 °F10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air 258 °C496 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75-1,-2
Vicat Softening Point  >= 230 °C
@Load 5.10 kg
>= 446 °F
@Load 11.2 lb
120°C/h; ISO 306
 >= 230 °C
@Load 5.10 kg
>= 446 °F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Oxygen Index 27 %27 %Method A; ISO 4589-2
Glow Wire Flammability Index 600 °C
@Thickness 2.00 mm
1110 °F
@Thickness 0.0787 in
IEC 60695-2-12
Shrinkage, MD 0.020 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.020 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Flow Direction Post-Molding, 150x105x3; ISO 294-4
Shrinkage, TD 0.040 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.040 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Molding, 150x105x3; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °Finjection molding; ISO 294
 280 - 300 °C536 - 572 °F
Mold Temperature 80.0 °C176 °Finjection molding; ISO 294
 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 6.00 hour2.00 - 6.00 hour
Moisture Content 0.030 - 0.12 %0.030 - 0.12 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram PlusTek PA303G50 Nylon 6.6, 50% Glass Fiber
Envalior Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber
Polyram PlusTek PA341G9 Nylon 6.6, 45% Glass Fiber
Polyram PlusTek RA301G8 Nylon 6.6 for Injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized
Polyram PlusTek RA303G7 Nylon 6.6, 35% Glass Fiber

PLANW9248 / 208047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.