MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Esenttia 130C80ND Impact Block Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Characteristics: Very high flow rate control reologhy impact block copolymer polypropylene; good impact/stiffness balance; ease of processing allows increased design freedom and higher productivity; excellent dimensional stability; good surface finish color; with nucleant and mold release additives

Recommended for: Injection molding of thin complex parts; housewares and consumer products.

Information provided by Esenttia by Propilco

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 130 g/10 min
@Load 2.16 kg,
Temperature 230 °C
130 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238B
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.7 MPa3440 psi50 mm/min; ASTM D638
Elongation at Yield 5.0 %5.0 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 1134 MPa164500 psi1.3 mm/min; ASTM D790-1A
Izod Impact, Notched 0.535 J/cm1.00 ft-lb/inASTM D256-A
Gardner Impact  10.0 J
@Temperature -30.0 °C
7.38 ft-lb
@Temperature -22.0 °F
ASTM D5420A
 20.0 J
@Temperature 23.0 °C
14.8 ft-lb
@Temperature 73.4 °F
ASTM D5420A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem CP1200B Homopolymer Polypropylene
PolyMirae Adstif EA5076 Polypropylene Copolymer
PolyMirae Moplen EP540V Polypropylene Copolymer
Total Lumicene® MR110MC2 Metallocene Random Copolymer Polypropylene, Injection Molding
Braskem H 152 Fiber Extrusion Polypropylene

PESEN048 / 184620

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.